Limit Oxygen Index Tester Test Procedure

The Limit oxygen index tester test requires the operator to calibrate the oxygen index meter before the test to ensure the accuracy of the test data. After calibration experiment, test requirement standard style for at least 15 root, respectively, in the style of any 50 mm at one end, insert the other end of the combustion on the tested style clip (the different forms, different thickness of the style, the test result is not).



The initial oxygen concentration was determined prior to the oxygen index test. If you are not sure, you can ignite the sample in the air and watch the combustion. Oxygen combustion soon, if the sample of the initial concentration of 18%, selected if sample from fire immediately after lighting the flame in the air, depending on the ignition easily from fire after out of selecting oxygen concentration of 25% or more of the oxygen concentration. Determine the oxygen concentration and begin the formal test.

First, open the oxygen and nitrogen cylinder valve door, adjust the pressure relief valve, the pressure is 0.2~ 0.3mpa. Adjust trace regulator, to stable the velocity of oxygen and nitrogen gas flow through the rotor flowmeter instructions, see the float on the surface, and adjust to the work place, at the same time check whether instrument gauge at 0.1 Mpa, otherwise, shall, in accordance with the provisions of regulation to the pressure, the N2 + O2 pressure gauge is not greater than 0.03 Mpa or does not display the pressure is normal, more than the pressure should check whether there is burning the column charcoal, gas road jams phenomenon, until meet the requirements. When the concentration of oxygen is tested or changed, the system must be flushed for 30s.

After the oxygen index measuring system is developed, it is used to ignite the sample with c, butane or natural gas. The flame length is 6~25mm. After the sample is ignited, the ignition source is removed immediately and the time is immediately started.

In the process of sample combustion, the combustion condition of the sample is observed. If the sample burns above 180s, or burns more than 50mm, the oxygen concentration is too high and must be reduced. The concentration of oxygen must be increased if the sample is extinguished before or 50mm before 180s. It is necessary to measure the percentage concentration of oxygen when the sample is extinguished at 180s or 50mm. And three times, the average of three times oxygen concentration was calculated.

Calculate: the oxygen index meter test frequency three times, and calculate the average, take the decimal place one.
The calculation formula of oxygen index is as follows :(OI)=O2 / (O2 +N2) *100%.

Note: volume percentage represents oxygen index.The Limit oxygen index test chamber test results were compared with the oxygen index of the reference material.

评论

此博客中的热门博文

How To Process The Elmendorf Tear Strength Test

The Elmendorf tear tester has been developed specially for the paper industry and is outstanding for simplicity of operation and high measurement accuracy. The exchangeable pendulum is equipped with a pneumatic sample clamp. The initiation and return of the pendulum, as well as sample cutting is completely automatic. The device is operated via an integrated touch screen, where the test method can be selected, specific settings can be adjusted, and, after the measurement, results and statistics can be  displayed.Each pendulum is supplied with the appropriate control weight so that, with the help of the service program, it can easily be checked for functionality and balance. The Elmendorf tear test Procedure:     Cotton fabric was taken.     Warp and weft direction of the fabric was identified.     Two strips were cut from the fabric in both directions having dimensions of 100 x 63.5 mm.     The sample was then fixed in the jaws of the ...

The Scratch Tester Working Principle From Qinsun LAB

The scratch test machine is used to evaluate the shear, scratch, planing, scraping and engraving performance of the material. Its applications include rigid organic materials, plastics and glass, and so on. The test parameters, such as the speed of scratches, the length of scratches, the distance between scratches and the number of lines, are the test equipment with strong applicability and convenience. scratch tester Working principle: Coating has three aspects: the action of protection, decoration, and hide the defects of products, and the three main hardness has a lot to do with paint, paint film hardness is said film one of the important properties of mechanical strength, is an important indicator of measuring coating product quality, and measure the coating hardness is an important index of the scratch resistance of determination; Coating good product in the process of packaging, transport and use will draw by hard brush, not row brush the paint film is often leave scratc...

Correct Use Of Color Assessment Cabinet

Observation Angle: The following points are all the facilities required for the Color Assessment Cabinet , and the viewing Angle will directly affect the evaluation results. According to international standards, there are only two observable angles that can be used. They are: A, zero light source and 45 degrees observation (0 °, 45 °), the light from zero (vertical) incident Angle on the sample, sample watchers from 45 degrees. B, light source and 45 ° inclined channel 45 degrees of light source, zero observation (0 °, 45 °), the layout must use specific 45 degrees of inclined (45 ° Fixed Angle table) making from 45 degrees of light source on the samples, sample watchers from zero (vertical). The location of the 45 ° light samples: Regardless of any of the above observation methods, it is important to note that the test sample is placed in the middle of the light box as far as possible to reduce the influence of the external light source. In addition, the most important thing...