anti-ultraviolet finishing agent HTUV100:Anti-UV finishing agent HTUV100 is manufactured by Herst International Group, which can be used for efficient and durable UV finishing of cotton, silk, wool, polyester, nylon and blended fabrics and to improve the fastness of some dyes. Clothing, beachwear, bath suits, casual clothes (T-shirts, shirts, hats, etc.), professional wear and tents, umbrellas, curtains and other UV shielding performance. The basic traits of HTUV100: Component: Triazepine Derivatives High Efficiency UV Absorbent Materials Appearance: light yellow liquid:Ionicity: Nonionic:PH: about 7:Solubility: miscible with water: Stability: in hard water, in the pH of 5 ~ 8 acid, alkali solution stability, easy to use Compatibility:

Safe use of anionic or cationic products The HTUV100 has the following characteristics:①, the polymer of the UV absorber, with excellent durability of the UV absorption and UV blocking shielding effect, the 180 ~ 400 nm band of ultraviolet absorption has a good absorption, reflection and scattering.
②, the amount of small, efficient and lasting effect, in the appropriate structure of the textile has a high UPF value.
③, and fiber affinity, thermal stability, suitable for a variety of processes, to the greatest degree of shielding UV
④, reactive products can be linked with the fiber, a very high resistance to washing and light stability, repeated washing and strong ultraviolet radiation effects are not decreased.
⑤, product versatility is good, easy to use. Applicable to finishing, coating, printing, spraying and high temperature suction method, padding process.

Property anti-ultraviolet finishing process screening:①, process recipe:
The test showed that the following formulation was used for the T40 / C60 45 * 45 110 * 76 fabric to achieve good UV protection.
Prescription (g / L): anti - UV finishing agent HTUV100 30
Crosslinking agent AF6900 30
②, process flow(90 ~ 80%) → drying (90 ~ 110 ℃) → high temperature tenter (170 ~ 190 ℃, 30 s). test results and discussion:
①, anti-ultraviolet performance test;
② Determination of formaldehyde content:
The use of GB / T2912.1 textile formaldehyde determination, anti-ultraviolet finishing agent HTUV100 finishing fabric formaldehyde content is 10 mg / kg, in full compliance with GBl8401 - 2001 "textile formaldehyde content limit" national mandatory standards.
③, irritating to the skin:
10% of the Japanese ear standard experimental rabbits with both sides of the spine were cut off, the 4% UV finishing agent HTUV100 application solution coated on the gauze, applied to the right side of the exposed skin.

24 h after the observation of the application of skin parts, no erythema and edema and other symptoms, according to the skin irritation strength grading standards, the anti-ultraviolet finishing agent application of the skin is a non-stimulating substance.acute oral toxicity:4% anti-ultraviolet finishing agent HTUV100 dose of l0000 mg / kg, the daily observation of animal poisoning performance, 10% of the anti-ultraviolet finishing agent HTUV100 application 40 pairs of fasting 16 h Kunming standard mice one-time oral administration, Day end of the experiment, each group of experimental animals throughout the course of the experiment, without any poisoning performance, diet and exercise were normal, no animal died. According to the acute toxicity classification standard, the 4% anti-ultraviolet finishing agent application liquid is the actual non-toxic substances.

评论

此博客中的热门博文

Classfication Of The Textile Testing

Textile testing is the term for a whole series of tests that examine the physical, mechanical and chemical properties of textiles. These tests are sometimes done before a textile goes into widespread use, or they're done on textiles arriving from other countries for sale in US markets. Countries like the United States have established standards for what should and should not be in textile products. Tests can show whether companies making textiles are in compliance or not. Many textile tests have many types. Some of them are physical tests, in which a sample of textile material is examined closely for feel and appearance. Such tests are done on individual fibers or strands of material and on yarns, threads made of several fibers twisted together. Textiles are subjected to light and other elements to see how they react. Some of these tests are done in a weather-ometer, a machine that tests for weathering and lightfastness of textiles. It's basically an enclosed box. Textiles...

How To Process The Elmendorf Tear Strength Test

The Elmendorf tear tester has been developed specially for the paper industry and is outstanding for simplicity of operation and high measurement accuracy. The exchangeable pendulum is equipped with a pneumatic sample clamp. The initiation and return of the pendulum, as well as sample cutting is completely automatic. The device is operated via an integrated touch screen, where the test method can be selected, specific settings can be adjusted, and, after the measurement, results and statistics can be  displayed.Each pendulum is supplied with the appropriate control weight so that, with the help of the service program, it can easily be checked for functionality and balance. The Elmendorf tear test Procedure:     Cotton fabric was taken.     Warp and weft direction of the fabric was identified.     Two strips were cut from the fabric in both directions having dimensions of 100 x 63.5 mm.     The sample was then fixed in the jaws of the ...

Standard Procedure Of Oxygen Index Test Methods

Oxygen index tester test methods, which describes the tendency of a material to sustain a flame, are widely used as a tool to investigate the flammability of polymers. They provide a convenient, reproducible, means of determining a numerical measure of flammability. A further attraction is that the test method uses inexpensive equipment and only requires a small sample size. These methods have been used to systematical investigate the relative flammabilities of fire-retarded materials, frequently comparing the effectiveness of fire-retardants and fire-retardancy mechanisms. The quintessential feature of oxygen-index methods is that the sample is burnt within a controlled atmosphere. The standard procedure is to ignite the top of the sample, using a gas flame which is withdrawn once ignition has occurred, and to find the lowest oxygen concentration in an upward flowing mixture of nitrogen and oxygen which just supports sustained burning. The criticality criterion typically tak...